Method for decreasing energy consumption during refining of...

D - Textiles – Paper – 21 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

92/34

D21D 1/12 (2006.01)

Patent

CA 1306378

ABSTRACT The energy consumption of a cellulosic fibrous material refiner is significantly reduced, while the capacity is maintained by reducing grinding frequency while increasing the retention time and power amplitude (edge bar load). The grinding frequency is maintained between about 200-2,000 Hz, preferably between about 300-900 Hz. The retention time is more than a second, being increased at least about 100 times compared to conventional disk refiners. The power amplitude is at least doubled. Retention time is increased by greatly increasing the retention volume by removing the majority (at least about 90%) of the steam at approximately the area that it is generated, minimizing the number of cutting elements, and disposing the grinding surfaces of the refiner so that they define a volume of revolution (e.g. a frusto-conical or cylindrical volume).

539688

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for decreasing energy consumption during refining of... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for decreasing energy consumption during refining of..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for decreasing energy consumption during refining of... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1233610

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.