ABSTRACT Blanketing of molten aluminum-lithium alloys is performed under a nontoxic and noncorrosive dichlorodifluoromethane containing gas atmosphere, which produces a thin self-passivating fluxing film on the melt surface. The blanketing atmosphere protects the melt from oxidation, burning, and lithium evaporation, improves alloy cleanliness and can be used in any furnace, transfer or casting operation. The blanketing atmosphere can be applied in the entire range of commercial or master aluminum-lithium alloys including pure lithium melts. The dichlorodifluoromethane concentration in the blanketing atmosphere can range from 0.05 to 100 vol% with the remainder being an inert gas such as argon.

550093

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Blanketing atmosphere for molten aluminum-lithium alloys or... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Blanketing atmosphere for molten aluminum-lithium alloys or..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Blanketing atmosphere for molten aluminum-lithium alloys or... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1312022

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.