3266OCA Abstract of the Disclosure An improved composite includes an improved polymer, specifically an improved poly(phenylene sulfide). The improved polymer is produced by an improved method including a polymerization phase, a recovery phase, a washing phase, and an optional air-curing phase. In the polymerization phase a low temperature cycle and a high temperature cycle are used. In a preferred recovery phase, solidified polymer is quenched with N-methyl-2-pyrrolidone. In the washing phase, the recovered solidified polymer is washed with a hot acidic solution and then hot water. In a preferred embodiment, the method produces substantially linear poly(phenylene sulfide) having a melt flow within the range of about 50 to about 200 grams per 10 minutes and an ash content of not greater than about 0.1 weight percent and a melt crystallization temperature of not less than about 347°F (175°C).

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Poly(arylene sulfide) and method of making, and article of... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Poly(arylene sulfide) and method of making, and article of..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Poly(arylene sulfide) and method of making, and article of... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1388504

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.