ABSTRACT A water-borne low adhesion backsize and release coating latex composition comprising: (a) about 5 to about 70 weight percent of a polymer comprising polymerized free radically polymerizable monomer of the formula CnH2n+1-P-CmH2m-X-CR1-CH2 wherein n is an integer of about 12 to about 20, P is a divalent polar linking group, X is a divalent linking group selected from the group consisting of -O?- and Image , m is an integer of about 2 to about 10, and R1 is selected from the group consisting of -H and -CH3, (b) about 30 to about 95 weight percent of an aqueous phase, and (c) about 0.05 to about 4 weight percent of an emulsifier, wherein particles of the polymer are stabilized by the emulsifier and dispersed within the aqueous phase. A method of making the latex and sheet materials coated therewith.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Water-borne acrylic low adhesion backsize and release... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Water-borne acrylic low adhesion backsize and release..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Water-borne acrylic low adhesion backsize and release... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1545834

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.