Method of preparing bismuth oxide superconducting wire

H - Electricity – 01 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

H01B 13/00 (2006.01) B21L 1/00 (2006.01) B21L 9/00 (2006.01) C01G 29/00 (2006.01) H01B 1/08 (2006.01) H01B 12/04 (2006.01) H01L 39/24 (2006.01)

Patent

CA 2092180

A manufacturing method wherein a metal sheath is filled with a powder having a composition such that the amounts of Sr, Ca and Cu are larger than conventional so that in addition to the 2223-phase of (Bi, Pb)-Sr-Ca-Cu the phase of Sr-Ca-Cu-O may be precipitated, and then, this metal sheath is subjected to a plastic working, a primary heat treatment, another plastic working, and a secondary heat treatment in this order. A pinning point based on the phase of Sr-Ca-Cu-O is introduced into the supercon- ductor of the obtained bismuth based oxide superconductive wire material, and thereby, the magnetic field characteristic of the critical current density is improved.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of preparing bismuth oxide superconducting wire does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preparing bismuth oxide superconducting wire, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing bismuth oxide superconducting wire will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1588716

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.