Separation and concentration method

C - Chemistry – Metallurgy – 22 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C22B 58/00 (2006.01) C22B 3/06 (2006.01) C22B 3/12 (2006.01) C22B 3/44 (2006.01) C25C 1/16 (2006.01)

Patent

CA 2295468

An object of the present invention is to make it possible to recover gallium and indium efficiently and at a low cost from solutions containing traces of gallium and indium. Jarosite is produced by performing a specific treatment on a solution obtained by a two-stage neutralization treatment during the zinc leached residue treatment step of wet zinc refining, or on another solution containing traces of gallium and indium; the gallium and indium are separated and concentrated; an alkali is added to the jarosite; and the gallium is separated and concentrated by leaching. Calcium hydroxide or magnesium hydroxide is optionally added to the jarosite leached solution to perform purifying, sulfuric acid is added to the purified solution. neutralization is performed, basic gallium sulfate is precipitated, the precipitate is subjected to alkali leaching, and the gallium in the leached solution is electrolytically extracted, yielding metallic gallium.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Separation and concentration method does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Separation and concentration method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Separation and concentration method will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1704742

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.