Method of making an asphalt coating

C - Chemistry – Metallurgy – 09 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C09D 195/00 (2006.01) B05D 1/02 (2006.01) B05D 1/28 (2006.01) C08J 11/06 (2006.01) E04B 1/64 (2006.01) E04G 21/28 (2006.01)

Patent

CA 2619211

The present invention involves the recycling of asphalt based roofing materials by comminuting the roofing material and subsequently separating a rock component from an asphalt component of the roofing material. The asphaltic component is separated into a feed stream having a mesh size of less than about 50 mesh while the rock component is separated into a feed stream having rocks in the size of 10 mesh or larger. A portion of the comminuted material may be recycled back for additional comminuting. The separated asphaltic component is placed in contact with the solvent to dissolve the asphalt in the asphaltic component providing a mixture of filler, fiber and dissolved asphalt. The liquid may then be applied to a surface of a wall to form a substantially continuous solidified film on the wall to provide waterproofing and an air barrier.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of making an asphalt coating does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making an asphalt coating, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making an asphalt coating will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1847178

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.