402/1, 402/301

C08F 220/52 (2006.01) C08F 8/32 (2006.01) C08F 8/48 (2006.01) G11B 7/253 (2006.01) G11B 7/26 (2006.01)

Patent

CA 2031783

ABSTRACT Intrinsically low birefringent molding polymers have a molten stress optic coefficient that is greater than or equal to -1000 Brewsters and less than or equal to +1000 Brewsters, a glass transition temperature of at least 140°C, and a water absorption (AH20 according to ASTM D570-81 after 24 hours immersion in water at 23°C) of less than 0.25 percent and comprise in polymerized form at least one structural component providing a positive melt homopolymer stress optic coefficient and at least one other structural component providing a negative melt homopolymer stress optic coefficient. They are particularly useful as substrates for optical storage discs. 36,077C-F

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Intrinsically low birefringent molding polymers, process for... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Intrinsically low birefringent molding polymers, process for..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Intrinsically low birefringent molding polymers, process for... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1945261

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.