CA 2695552

Polyethylene wax having a number average molecular weight of from 1,000 to 10,000 and a molecular weight distribution of from 2 to 4 may be produced using a phosphinimine catalyst under "forced" solution polymerization conditions. The "forced" conditions include high polymerization temperatures; comparatively low catalyst efficiencies and very high ethylene conversions. These "forced" conditions may be achieved by operating the reactor at a temperature of between 190° C and 250° C, using a high catalyst concentration and high ethylene conversion. Using these conditions, polyethylene wax may be produced in the absence of hydrogen.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing low molecular weight wax does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing low molecular weight wax, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing low molecular weight wax will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1948861

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.