Method of producing aluminum alloy heat-exchanger

B - Operations – Transporting – 21 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

B21D 53/02 (2006.01) B21C 37/22 (2006.01) B23P 15/26 (2006.01) C22F 1/04 (2006.01) C22F 1/043 (2006.01)

Patent

CA 2080865

ABSTRACT A method of producing aluminum alloy heat-exchanger is disclosed, wherein, upon producing aluminum alloy heat-exchanger by soldering technique, it is retrained for 10 minutes to 30 hours at 400 to 500°C after the finish of heating for soldering. It is better to retain the heat-exchanger during cooling after the finish of heating for soldering or the heat-exchanger cooled to 150°C or lower after the finish of heating for soldering for 10 minutes to 30 hours at 400 to 500°C and further it is preferable to cool at a cooling velocity of not slower than 30°C/min across a temperature range from 200-C to 400°C after said reteinment. Excellent thermal efficiency, high strength and excellent corrosion resistance can be achieved.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing aluminum alloy heat-exchanger does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing aluminum alloy heat-exchanger, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing aluminum alloy heat-exchanger will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1973432

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.