C22C 38/18 (2006.01) C21D 6/00 (2006.01) C21D 8/10 (2006.01) C21D 9/08 (2006.01) C22C 38/40 (2006.01) C22C 38/58 (2006.01) F16L 9/02 (2006.01)
Patent
CA 2249964
A martensitic stainless steel pipe comprises, on the weight basis, C:0.005 to 0.2%, Si: 1% or below, Mn: 0.1 to 5%, Cr: 7 to 15%, and Ni: 0 to 8%, wherein a wall thickness t (mm) and contents of C and Cr satisfy the relationship represented by the following equation (1). t (mm) ~ exp{5.21 -18.1C (%) - 0.0407Cr (%)} ...... (1) The steel pipe can be made by employing water quenching as a quenching method.
Amaya Hisashi
Kondo Kunio
Ueda Masakatsu
Gowling Lafleur Henderson Llp
Sumitomo Metal Industries Ltd.
LandOfFree
Martensitic stainless steel pipe and method for... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Martensitic stainless steel pipe and method for..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Martensitic stainless steel pipe and method for... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1994173