ABSTRACT OF THE DISCLOSURE: An electrical contact material obtained through inter- nally oxidizing a silver alloy which is the solid solution with 3 to 11 weight percent of tin and other solute metal element(s). The alloy material is improved of its contact resistance by dif- fusing into the silver matrix 0,1 to 5 weight percent of metals having a decomposition and sublimation temperature lower than the melting point of silver and then by internally oxidizing the material.

323207

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Electrical contact materials containing internally oxidized... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Electrical contact materials containing internally oxidized..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Electrical contact materials containing internally oxidized... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-212932

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.