CA 1110142
ABSTRACT OF THE DISCLOSURE Weld brittleness of silicon-iron can be reduced without loss of excellent magnetic properties by limiting the sulfur content to not more than 0.018 per cent and using copper as a partial substitute for sulfur as a normal grain growth inhibitor during the final texture-developing anneal.
311266
Company General Electric
Eckersley Raymond A.
LandOfFree
Method of producing silicon-iron sheet material with copper... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of producing silicon-iron sheet material with copper..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing silicon-iron sheet material with copper... will most certainly appreciate the feedback.