This invention provides a joining area (10) and method between copper (2) and stainless steel or titanium (3), as well as the permanent cathode (1) obtained, where said joining area (10) is made of a first zone (101) of a copper-nickel (Cu-Ni) alloy, an intermediate zone (102) with a mostly nickel alloy or pure nickel and a second zone (103) made of a stainless steel-nickel alloy, which is the result of the participating materials being cast in an arc welding process, for example TIG, MIG or manual arc using electrodes of nickel as welding contributor between said materials and their space arrangement, that is to say, leaving a separation between the materials when performing the welding process, thus ensuring as follows: a) greater tensile strength, b) a substantial improvement of corrosion resistance of the joint welding, and c) improvement of conductibility, which can be improved still further by modifying the straight design of the conducting bar by providing it with the "horn"-type shape.
Mouthon Horacio Rafart
Rosende Antonio Carracedo
Gowling Lafleur Henderson Llp
Industria Proveedora de Partes Metalurgicas Limitada
LandOfFree
A corrosion resisting joining area and method between... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with A corrosion resisting joining area and method between..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and A corrosion resisting joining area and method between... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1786818