A method of densifying crosslinked fibers

D - Textiles – Paper – 04 – H

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

D04H 1/54 (2006.01) A61F 13/15 (2006.01) A61L 15/28 (2006.01) D21H 25/00 (2006.01) A61F 13/48 (1990.01)

Patent

CA 2107214

2107214 9215741 PCTABS00016 A method is disclosed for the densification of crosslinked fibers having a crosslinking agent loading level of from about 2.5 molar to about 5 molar %. The crosslinked fibers are compressed from an initial density of from about 0.02 g/cc to about 0.04 g/cc to a second density of from about .20 g/cc to about 1.00 g/cc by either the simultaneous or sequential application of heat and pressure. The surface temperature of the press is typically between about 60 ·C to about 180 ·C. The compression force for the air laid or wet laid webs is in the range of about 800 psi to about 115,000 psi. Densifying the crosslinked fiber in this manner produces a compressed web having enhanced absorbent capacities of from about 21 g/g to about 15 g/g.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

A method of densifying crosslinked fibers does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with A method of densifying crosslinked fibers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and A method of densifying crosslinked fibers will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1573146

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.