ABSTRACT A cast iron alloy composition comprising 2.5-3.5% carbon, 0.5-1.0% manganese, 0.25-1.5% silicon, 13-19% chromium, 0.8-3.0% nickel, balance essentially iron which is machinable in the annealed condition and abrasion resistant in the hardened condition. The alloy may be annealed by furnace cooling, at a rate between 100°C and 350°C/hr, from the austenitizing tempera- ture, and hardened by air cooling from the austenitizing temper- ature.

371420

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Abrasion resistant, machinable white cast iron does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Abrasion resistant, machinable white cast iron, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Abrasion resistant, machinable white cast iron will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-582813

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.