C-4063 ACCELERATED WHISKER GROWTH ON IRON-CHROMIUM-ALUMINUM ALLOY FOIL Abstract of the Disclosure An accelerated method for growing oxide whiskers on aluminum-containing stainless steel foil comprises heating the foil in air at an initial temperature suitably less than 960°C, preferably between 900°C and 950°C, to initiate whisker growth and thereafter increasing the temperature to above 960°C, preferably between 960°C and 990°C, to continue whisker growth at an accelerated rate and thereby reduce the time and processing expense required to grow mature whiskers of a desired size.

606241

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Accelerated whisker growth on iron-chromium-aluminum alloy foil does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Accelerated whisker growth on iron-chromium-aluminum alloy foil, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Accelerated whisker growth on iron-chromium-aluminum alloy foil will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1300394

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.