- 21 - Abstract of the Disclosure Advanced High Strength Single Crystal Superalloy Compositions A superalloy composition and single crystal articles of the composition are described. The broad range is 3-12% Cr, 0-3% Mo, 3-10% W, 0-5% Re, 6-12% Ta, 4-7% Al, 0-15% Co, 0-0.045% C, 0-0.02% B, 0-0.1% Zr, 0-0.8% Hf, 0-2% Nb, 0-1% V, 0-0.7% Ti, 0-10% (Ru+Rh+Pd+Os+Ir+Pt), balance essentially Ni. An equation is presented to select the most useful specific compositions from within this range. An exemplary preferred composition is 5.0% Cr, 10.0% Co, 2.0% Mo, 6.0% W, 3.1% Re, 5.6% Al, 9.0% Ta, 0.1% Hf, balance essentially Ni.

499551

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Advanced high strength single crystal superalloy compositions does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Advanced high strength single crystal superalloy compositions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Advanced high strength single crystal superalloy compositions will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1285830

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.