Air jet-texturing process for production of low- shrinkage...

D - Textiles – Paper – 02 – G

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

28/34

D02G 3/00 (2006.01) D02G 1/16 (2006.01)

Patent

CA 1148728

ABSTRACT OF THE DISCLOSURE A process is disclosed for producing an air jet textured polyester yarn having a low dry heat shrinkage. The process comprises the steps of: (a) cold drawing a spin-oriented polyester yarn at a draw ratio of from 1.3 to 2.0; (b) preheating the drawn yarn at substantially constant length; (c) feeding the yarn to an air jet at a 10% to 40% overfeed; (d) jet-texturing the yarn with the air jet; (e) drawing the jet-textured yarn at a draw ratio of 1.04 to 1.12; and (f) winding up the resulting air jet-textured yarn. In an embodiment of the process a step of post- heating the jet-textured yarn is included between step (e) and step (f) in order to reduce the size of the surface loops and to improve the stability of the jet-textured yarn.

367513

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Air jet-texturing process for production of low- shrinkage... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Air jet-texturing process for production of low- shrinkage..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Air jet-texturing process for production of low- shrinkage... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-499676

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.