Alloys resistant to stress-corrosion cracking in leaded high...

C - Chemistry – Metallurgy – 22 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

CPC

75/112

IPC codes

C22C 19/00 (2006.01) C22C 19/05 (2006.01)

Type

Patent

Patent number

CA 892489

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Alloys resistant to stress-corrosion cracking in leaded high... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Alloys resistant to stress-corrosion cracking in leaded high..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Alloys resistant to stress-corrosion cracking in leaded high... will most certainly appreciate the feedback.