Annealed polydioxanone polymer surgical device and method...

A - Human Necessities – 61 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

167/323, 18/49

A61B 17/08 (2006.01) A61L 17/10 (2006.01) A61L 17/14 (2006.01) A61L 31/06 (2006.01) C08G 63/664 (2006.01)

Patent

CA 1196158

ABSTRACT The strength and functional integrity of a thermally formed surgical device made from a polymer of p-dioxanone are improved by drying the thermally formed device at a temperature of less than 30°C to remove subs- tantially all moisture from the device. The dried device is then heated in a dry, inert atmosphere at a temperature of 50°C to 90°C for a period of time sufficient to increase the crystallinity of the device to at least 43%. The resultant new product comprises a thermally formed sur- gical device made from a polymer of p-dioxanone having a density of at least 1.384 grams per cubic centimeter and a crystallinity of at least 43%. The new surgical devices of the invention also have improved audible and tactile properties as well as improved shelf-life.

408213

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Annealed polydioxanone polymer surgical device and method... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Annealed polydioxanone polymer surgical device and method..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Annealed polydioxanone polymer surgical device and method... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1239918

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.