C - Chemistry – Metallurgy – 25 – D
Patent
C - Chemistry, Metallurgy
25
D
204/11.5, 204/24
C25D 11/08 (2006.01) B41N 3/03 (2006.01) C25D 11/04 (2006.01)
Patent
CA 1236421
ABSTRACT OF THE DISCLOSURE In the process for the anodic oxidation of mechanically, chemically and/or electrochemically roughened aluminum or of one of its alloys, an aqueous electrolyte, which is free from H2SO4 and contains H3PO4 and Al+3 ions is used. The process parameters are: an electrolyte content of 25 g/l to 500 g/l of H3PO4 and at least 5 g/l of Al+3 ions, a treatment time of 5 seconds to 500 seconds, a current density of 1 A/dm2 to 30 A/dm2 and a temperature of 35°C to 95°C. The Al+3 ion source in particular is a salt of aluminum having a phosphoroxo anion, such as AlPO4. The material prepared in accord- ance with this invention is preferably employed as a support material for offset printing plates which carry a radiation-sensitive layer.
478562
Fetherstonhaugh & Co.
Hoechst Aktiengesellschaft
LandOfFree
Anodic oxidation of aluminum in phosphoric acid containing... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Anodic oxidation of aluminum in phosphoric acid containing..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Anodic oxidation of aluminum in phosphoric acid containing... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1272445