C - Chemistry – Metallurgy – 08 – G
Patent
C - Chemistry, Metallurgy
08
G
400/102, 154/123
C08G 63/13 (2006.01) B32B 5/20 (2006.01) C08G 18/42 (2006.01) C08G 63/42 (2006.01)
Patent
CA 2012297
A polyester polyol composition is prepared by (1) reacting 5 to 40 percent tall oil fatty acids, (b) 20 to 80 percent dimethyl terephthalate process residue and (c) 20 to 60 percent polyhydric alcohol, based on the weight of the reaction mixture, in the presence of an esterification/transesterification catalyst while continuously removing water and methanol that are formed during the reaction, to form a first reaction product containing residual carboxylic acid functionality and (2) reacting 1 to 25 percent of at least one alkylene carbonate, or an equimolar amount of at least one alkylene oxide, with the residual carboxylic acid functionality in the presence of a catalyst. The preferred alkylene carbonate/oxide is ethylene or propylene (or a mixture thereof) carbonate/oxide. A foamed laminate made from the polyester polyol has reduced surface friability and faster rates of cure.
Lange Scott Frederick
Trowell John Maynard
Cape Industries
Smart & Biggar
LandOfFree
Aromatic polyester polyols from dimethyl terephthalate... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Aromatic polyester polyols from dimethyl terephthalate..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aromatic polyester polyols from dimethyl terephthalate... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1956807