C - Chemistry – Metallurgy – 04 – B
Patent
C - Chemistry, Metallurgy
04
B
C04B 35/645 (2006.01) B22F 3/12 (2006.01) B22F 5/00 (2006.01) B23P 15/28 (2006.01) C04B 35/56 (2006.01) E21B 10/08 (2006.01) E21B 10/42 (2006.01) E21B 10/46 (2006.01)
Patent
CA 2603458
A sintered body for cutting tools that includes hard particle phase comprising a plurality of hard particles, wherein at least a portion of the hard phase particles comprise a coating deposited by atomic layer deposition disposed thereon; and a binder phase is disclosed. The hard particles that may be included in the sintered bodies may include tungsten carbide, diamond, and boron nitride particles.
Belnap J. Daniel
Keshavan Madapusi K.
Shen Yuelin
Yao Xian
Yu Feng
Smart & Biggar
Smith International Inc.
LandOfFree
Atomic layer deposition nanocoatings on cutting tool powder... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Atomic layer deposition nanocoatings on cutting tool powder..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Atomic layer deposition nanocoatings on cutting tool powder... will most certainly appreciate the feedback.