ABSTRACT OF THE DISCLOSURE This invention relates to a bare electrode for welding of low temperature steel. More particularly, the invention relates to a welding bare electrode of a diameter of at least 3.0 mm for use in a large current gas shielded arc welding process in which steel for low temperature use is welded by a welding current of at least 500 A in a shielding gas composed mainly of an inert gas such as Ar, He or the like, said electrode comprising up to 0.12 % C, up to 0.8 % Si, up to 3.0 % Mn, up to 0.25 % Ti and at least one member selected from the group consisting of up to 4.0% Ni, up to 0.8 % Cr and up to 1.0 % Mo and the carbon equivalent (Ceq), represented by the following formula, of said electrode being up to 0.60 %: Ceq = C + 1/6Mn + 1/24Si + 1/40Ni + 1/5Cr + 1/4 Mo wherein each element denotes the content, % by weight, of the element.
240581
Aida Isao
Godai Tomokazu
Nakagaki Masatoshi
Kobe Steel
LandOfFree
Bare electrode for welding of low temperature steel does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Bare electrode for welding of low temperature steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Bare electrode for welding of low temperature steel will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1152148