CA 1095540
ABSTRACT OF THE DISCLOSURE: A binding agent based on ground cement clinker having a specific surface area greater than 150 m2/kg, setting at tempera- tures below +8°C and containing as admixtures water and at least 0.0025 weight percent of a compound based on lignosulfonates, calculated on the total amount of cement clinker, and, optionally, further admixtures necessary for the preparation of mortars and concretes, which consists of 5 to 99.94 weight percent of cement clinker having a specific surface area of 250 to 3000 m2/kg and containing 5 to 95 weight percent of particles of a size of up to 5 micrometers, and of 0.05 to 80 weight percent of formation water, calculated on the total amount of cement clinker. The binding agent of the invention may be used in a broad temperature ranging from +8°C to -40°C.
299913
Bazantova Zdenka
Kolar Karel
Novotny Jaroslav
Satava Vladimir
Skvara Frantisek
Ceskoslovenska Akademie Ved
Robic Robic & Associes/associates
LandOfFree
Binding agent based on cement clinker does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Binding agent based on cement clinker, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Binding agent based on cement clinker will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-32120