The present invention relates to a brass alloy having superior stress corrosion comprising: 59.0-64.0wt% Cu, 0.6-1.2wt% Fe, 0.6-1.0wt% Mn, 0.4-1.0wt% Bi, 0.6-1.4wt% Sn, at least one element selected from Al, Cr and B, the balance being Zn and unavoidable impurities, wherein the content of Al is 0.1-0.8wt%, the content of Cr is 0.01-0.1 wt%, the content of B is 0.001-0.02wt%. The alloy according to the present invention does not contain toxic elements such as lead and antimony, has superior corrosion resistance and good cuttingability and is suitable for the accessories in the potable water supply systems produced by casting, forging and extruding.
Hu Zhenqing
Xu Chuankai
Zhang Siqi
Smart & Biggar
Xiamen Lota International Co. Ltd
LandOfFree
Brass alloys having superior stress corrosion resistance and... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Brass alloys having superior stress corrosion resistance and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Brass alloys having superior stress corrosion resistance and... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1404128