ABSTRACT OF THE DISCLOSURE A catalyst pretreat procedure wherein a copper, selenium, or sulfur promoted platinum-iridium catalyst, preferably a platinum-iridium-selenium catalyst, is contacted with dry hydrogen at a temper- ature ranging from about 600°F - 1000°F, at a hydrogen partial pressure ranging from about 1 - 40 atmospheres at a flow rate sufficient to maintain the moisture level below about 500 parts per million parts by volume of gas in the exit gas stream, for a period of time ranging at least about 16 hours, preferably at least 16 hours to about 200 hours. Treatment of these catalysts at such conditions will provide a selectivity advantage ranging from about 1 to 2 (LV%) higher than a catalyst otherwise similar but not pretreated in this manner.

427312

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Catalytic reforming process does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Catalytic reforming process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Catalytic reforming process will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1217095

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.