Chemical Milling of High Tungsten Content Superalloys Abstract Chemical milling of cast superalloys having high tungsten contents is advantageously accomplished with an etchant which consists by volume percent of 40-60 concentrated HNO3, 0.6-0.8 concentrated HF, 40-70 H2O, with which is included at least 0.008 moles/liter CuSO4 and 0.0016-0.025 moles/liter FeCl3. Preferably the molar ratio of CuSO4 to FeCl3 is 2:1 and etching is accomplished in the range 50-80°C.
386180
Fishter Robert E.
Lada Henry
Manty Brian A.
Swabey Ogilvy Renault
United Technologies Corporation
LandOfFree
Chemical milling of high tungsten content superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Chemical milling of high tungsten content superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Chemical milling of high tungsten content superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-476771