Abstract of Disclosure A method is provided for separating chromium from lateritic ore. The ore which generally also contains nickel and cobalt along with other metal values is leached with a strong sulfuric acid solution of about 10 to 30 normal concen- tration at an acid to ore ratio of at least 3:1 by weight. The leaching is carried out at a temperature of at least 100°C ranging as high as about 300°C at above atmospheric pressure. An oxidant, such as manganese dioxide, is preferably added to oxidize the chromium to the hexavalent state, the manganese dioxide, or its equivalent, being advantageous in improving the chromium yield at the lower end of the leaching temperature range.

233973

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Chromite recovery from chromite-bearing ore does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Chromite recovery from chromite-bearing ore, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Chromite recovery from chromite-bearing ore will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-154237

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.