COBALT-BASE SUPERALLOY ABSTRACT OF THE DISCLOSURE Disclosed is a cobalt-base superalloy containing about 32% cobalt, 8% nickel, 26.5% chromium, 2.5% tungsten, 5% niobium, about 1% each maganese and silicon, about .4% carbon, and the balance about 23% iron plus incidental impurities and modifiers normally found in alloys of this class. The alloy is readily processed in the form of wrought products, castings, metal powder and all forms of welding and hardfacing materials. The outstanding characteristics of the new alloy include the resistance to cavitation erosion and galling, low cost and minimal use of strategic metals.
397576
Crook Paul
Cabot Corporation
Marcoux & Sher Swabey Mitchell Houle
LandOfFree
Cobalt-base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Cobalt-base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Cobalt-base superalloy will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1303914