4680-362 COBALT-CHROMIUM SUPERALLOY Abstract An oxide dispersion strengthened cobalt-chronium superalloy produced by mechanical alloying containing a refractory oxide, preferably yttrium oxide, and characterized by excellent corrosion resistance, high fatigue strength and high temperature stability; and prostheses formed from said superalloy.