C04B 35/52 (2006.01) C04B 35/58 (2006.01)
Patent
CA 2124167
A composite material includes boron carbide and titanium diboride in a volume ratio B4C/TiB2 of from 90:10 to 10:90 parts and a proportion of elemental carbon greater than 2% by weight up to a maximum of 50% by weight, based on the boron carbide content. The composite material has a density greater than 92% TD, a hardness HK 0.1 greater than 2300, a four-point flexural strength greater than 400 MPa and a fracture toughness greater than 3.5 MPa.sqroot.m. The composite material is suitable for producing wear-resistant components or cutting tools.
Schwetz Karl-Alexander
Sigl Lorenz
Thaler Hubert
Elektroschmelzwerk Kempten Gmbh
Esk Ceramics Gmbh & Co. Kg
Mcfadden Fincham
LandOfFree
Composite materials based on boron carbide, titanium... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Composite materials based on boron carbide, titanium..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Composite materials based on boron carbide, titanium... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1478035