C - Chemistry – Metallurgy – 23 – F
Patent
C - Chemistry, Metallurgy
23
F
C23F 15/00 (2006.01) F16L 58/00 (2006.01) F17D 5/00 (2006.01)
Patent
CA 2417739
A method of reducing stress corrosion cracking in a member made of metal, such as a pipe, comprises applying a load to the member to prevent stress corrosion cracking.
Bereskin & Parr
The Governors Of The University Of Alberta
LandOfFree
Control of stress corrosion cracking growth by operational... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Control of stress corrosion cracking growth by operational..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Control of stress corrosion cracking growth by operational... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1847510