Dimples, preferably 40 to 200 µm in average depth and 0.5 to 3 mm in diameter of circle equivalent, are formed on the peripheral surface of a cooling drum, adjacent to each other at the rims of the dimples; and fine humps (preferably, fine humps 1 to 50 µm in height and 5 to 200 µm in diameter of circle equivalent on the surfaces of the dimples and/or fine humps 1 to 50 µm in height and 30 to 200 µm in diameter of circle equivalent at the rims of the dimples), fine holes (preferably, fine holes 5 µm or more in depth and 10 to 200 µm in diameter of circle equivalent), or fine unevenness (preferably, fine unevenness 1 to 50 µm in average depth and 10 to 200 µm in diameter of circle equivalent) are formed at the rims and/or on the indented surfaces of said dimples.
Des corps creux, notamment des corps creux ayant chacun une profondeur moyenne de 40 à 200 mu m et un diamètre équivalent à 0,5 3 mm, sont formés sur la surface périphérique d'un tambour de refroidissement, ces corps creux étant adjacents au niveau de leurs extrémités lors du moulage. Sur/dans ces extrémités et/ou les surfaces desdits corps creux sont formés de minuscules saillies (de préférence, des saillies de 1 50 mu m de hauteur et de 5 200 mu m de diamètre sur la surface des corps creux, et de 1 50 mu m de hauteur et de 30 200 mu m de diamètre sur les extrémités des corps creux), de petits puits (de préférence, des puits d'au moins 5 mu m de profondeur et 10 200 mu m de diamètre) ou de minuscules irrégularités (de préférence, des irrégularités de 1 50 mu m de profondeur et de 10 200 mu m de diamètre).
Hamada Naoya
Ishimaru Eiichiro
Izu Tadahiro
Kurisu Yasushi
Maruki Yasuo
Goudreau Gage Dubuc
Nippon Steel Corporation
LandOfFree
Cooling drum for thin slab continuous casting, processing... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Cooling drum for thin slab continuous casting, processing..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Cooling drum for thin slab continuous casting, processing... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1655578