Copolymers of polyaspartic acid which are suitable for the inhibition of scale deposition were obtained by reacting maleic acid, an additional polycarboxylic acid and ammonia in a stoichiometric excess, at 120-350°C, preferably 180-300°C, to provide copolymers of polysuccinimide. In a second embodiment, a polyamine was added to the reaction mix. These intermediate polysuccinimide copolymers could then be converted to the salts of copolymers of polyaspartic acid by hydrolysis with a hydroxide. Such copolymers are useful in preventing deposition of scale from water and find applications in treating water. Other applications include scale prevention additives for detergents. In addition, such copolymers inhibit dental tartar and plaque formation.
Calton Gary J.
Wood Louis L.
Aktiengesellschaft Bayer
Fetherstonhaugh & Co.
Lanxess Deutschland Gmbh
LandOfFree
Copolymers of polyaspartic acid and polycarboxylic acids and... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Copolymers of polyaspartic acid and polycarboxylic acids and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Copolymers of polyaspartic acid and polycarboxylic acids and... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1396437