CA 2032993
IMPROVED COPPER-NICKEL-SILICON-CHROMIUM ALLOY Abstract of the Disclosure A copper-nickel-silicon-chromium alloy having the combination of high hardness and high electrical conductivity. The alloy is composed by weight of 8.5% to 11.5% nickel, in an amount sufficient to provide a nickel-silicon ratio of 3.4 to 4.5, 0.5% to 2.0% chromium, and the balance copper. The alloy is heat treated by initially heating the alloy to a solution temperature and is thereafter quenched. The quenched alloy is then aged to precipitate the metal silicides. Because of the specific ratio of nickel to silicon, the heat treated alloy develops during heat treatment a hardness in excess of 30 Rockwell C and an electrical conductivity in excess of 24% of pure copper.
Ampco Metal Manufacturing Inc.
Borden Ladner Gervais Llp
Ingerson Quentin F.
LandOfFree
Copper-nickel-silicon-chromium alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Copper-nickel-silicon-chromium alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Copper-nickel-silicon-chromium alloy will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-2064962