CA 1136652

ABSTRACT OF THE DISCLOSURE The present demolition agent for brittle materials is prepared by pulverizing a clinker which is obtained by mixing a calcareous material, a siliceous material and gypsum at the molar ratio of CaO/SiO2 = 5.0 - 14.4 and CaSO4/SiO2 = 0.13 - 1.19 and burning the mixture under an oxidizing atmosphere to 1350 - 1550 °C. The main components of the clinker thus obtained consist of 24 - 65 % by weight of 3CaO.SiO2 crystals, 30 - 60 % by weight of CaO crystalline particles and ? - 17 % by weight of CaSO4, wherein more than 50% by weight of said CaO crystalline particles is included in the large 3CaO.S1O2 crystals grown. The present demolition agent is used to break brittle materials by means of the expansive stress of aqueous slurry of the demolition agent poured into the hole of the brittle materials.

348072

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Demolition agent for brittle materials does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Demolition agent for brittle materials, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Demolition agent for brittle materials will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-808880

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.