The refractory material applied to an electric arc furnace runner is 85 to 95 wt. percent alumina, and 5 to 15 wt. percent aqueous sodium silicate. The heat from molten metal being processed is transmitted to the refractory material of the present invention by contact of the molten metal with the refractory material or by transmission of heat to the refractory material so as to sinter at least a portion of the refractory material and form a solid barrier to the flow of molten metal through the refractory. After the molten metal has been processed and no longer contacts the refractory material, the refractory material can have a portion which is free of water and remains in the form of a powder.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Electric arc furnace runner and method of forming an... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Electric arc furnace runner and method of forming an..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Electric arc furnace runner and method of forming an... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1631018

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.