A plate-, foil- or web-shaped workpiece of aluminum or an alloy thereof is subjected, in an electrolyte bath, to an alternating current at a frequency of 0.1 to 25 Hz. During the AC treatment, an anodic potential is imposed on the workpiece, in the range of 0 to 5 Volts. The total charge input is 10 to 60 kC/m2. Prior to the electrochemical graining, the workpiece is mechanically grained. After the graining steps, an etching treatment as well as an anodical oxidation and, thereafter, a hydrophilization are performed.
Fetherstonhaugh & Co.
Hoechst Aktiengesellschaft
LandOfFree
Electrochemical graining method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Electrochemical graining method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Electrochemical graining method will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1574616