CA 2330071

A laminar structure comprised of at least two layers (16, 20) of glass and a sheet (18) of plasticized PVB con-taining an adhesion control additive is provided wherein the difference in adhesion between the PVB interlayer and the glass due to glass orientation is minimized by includ-ing a leveling agent in the bulk or on the surface of the sheet of plasticized PVB or by coating the leveling agent onto the glass prior to laminating.

Cette invention concerne une structure laminaire qui comprend au moins deux couches (16, 20) de verre ainsi qu'une feuille (18) d'un PVB plastifié contenant un additif de modification de l'adhérence. La différence d'adhérence entre la couche intermédiaire de PVB et le verre, qui est due à l'orientation du verre, est minimisée en introduisant un agent de nivellement dans la masse ou à la surface de la feuille de PVB plastifié ou, encore, en appliquant l'agent de nivellement sur le verre avant de le stratifier.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Eliminating adhesion difference due to glass orientation in... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Eliminating adhesion difference due to glass orientation in..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Eliminating adhesion difference due to glass orientation in... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1984626

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.