402/364

C08G 73/00 (2006.01) C06B 45/10 (2006.01) C07C 243/02 (2006.01) C08G 63/685 (2006.01)

Patent

CA 1320612

ABSTRACT Poly(diethylene glycol-4,7-dinitrazadecane-dioate), (P-DEND), is synthesized by the Michael addition of ethylene dinitramine to methyl acrylate to yield the intermediate compound dimethyl-4,7-dinitrazadecane-dioate (DMDND). DMDND is reacted for a period of about 18 hours with diethylene glycol (DEG) at about 85°C in presence of a p-toluenesulfonic acid catalyst to yield P-DEND. The product (P-DEND) is purified by passing it through a silica gel column using methylene chloride as solvent. The average molecular weight of P-DEND ranges from about 1500-2000. P-DEND is shown to be compatible with stabilized nitroglycerin for use as an energetic polymer binder for high performance propellants.

553707

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Energetic polymer, p-dend does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Energetic polymer, p-dend, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Energetic polymer, p-dend will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1166968

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.