FATIGUE-RESISTANT NICKEL-BASE SUPERALLOYS Abstract of the Disclosure New ?' strengthened nickel-base superalloy compo- sitions are described that, when forged and properly heat treated, demonstrate superior resistance to fatigue crack growth accompanied by very good high temperature properties. Parts now can be fabricated (e.g., using conventional cast and wrought processing) from these alloys without encounter- ing difficulty in forging.
502406
Company General Electric
Eckersley Raymond A.
LandOfFree
Fatigue-resistant nickel-base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fatigue-resistant nickel-base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fatigue-resistant nickel-base superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1215416