Fibre reinforced superalloys and process for making same

C - Chemistry – Metallurgy – 30 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

CPC

75/1.2, 148/55.2

IPC codes

C30B 21/02 (2006.01)

Type

Patent

Patent number

CA 1041322

Description

ABSTRACT OF DISCLOSURE Composite materials for use in the manufacture of metallic objects comprising a matrix of a complex refractory superalloy and embedded in said matrix filiform particles of carbide and in the matrix a fine precipitation of carbide of the same nature as the one of the filiform particles.

Application Number

205587

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Fibre reinforced superalloys and process for making same does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Fibre reinforced superalloys and process for making same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fibre reinforced superalloys and process for making same will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-849433

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.