204/185

C25C 1/00 (2006.01) C25C 1/12 (2006.01)

Patent

CA 1133850

ABSTRACT OF THE DISCLOSURE A process and apparatus are disclosed for continuously manufacturing metallic anodes from molten metal. The process comprises continuously casting the molten metal in an inclined moulding cavity formed by two movable belts and by two movable side dams so as to produce a metallic strip, and by cutting the hot strip, when it has left the moulding cavity, with at least one plasma torch along a profile such that anodes with a low waste coefficient and without deformation are obtained (figure 1). This process allows the production of anodes made of very impure copper whereas conventional processes are limited to the production of anodes of relatively pure copper. This divisional application is particularly directed to a flat anode with a low waste coefficient. The two faces of the anode have substantially the same smoothness.

377651

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Flat anode having low waste coefficient does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Flat anode having low waste coefficient, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Flat anode having low waste coefficient will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1115399

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.