Coal fines are flocculated from an aqueous suspension by adding an anionic polyelectrolyte, a soluble calcium salt, and a cationic polyelectrolyte to the suspension. The anionic polyelectrolyte is preferably a high charge density, high molecular weight acrylic acid/acrylamide copolymer or a high charge density high molecular weight terpolymer of acrylic acid/methacrylic acid/ethylacrylate. The cationic polyelectrolyte is preferably a high molecular weight, low charge density dimethylamino methylmethacrylate methyl chloride quaternary ammonium salt/acrylamide copolymer, an N,N dimethyl 2 hydroxy propyl imine homopolymer of low molecular weight, a diallyl dimethyl ammonium chloride polymer, or ter polyepichlorohydrin dimethyl amine.

602912

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Flocculation of coal fines with poly-electrolytes and... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Flocculation of coal fines with poly-electrolytes and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Flocculation of coal fines with poly-electrolytes and... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1244528

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.