-14- Forging Process for Superalloys Abstract Forging processes are described for cast superalloys. The forgeability of superalloy materials is improved by the development of overaged microstructure. The total forging process is usually performed in a series of steps with intervening heat treatments to reform the overaged microstructure.
464974
Brown Edgar E.
Malley David R.
Paulonis Daniel F.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
United Technologies Corporation
LandOfFree
Forging process for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Forging process for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Forging process for superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1277761