ABSTRACT OF THE DISCLOSURE A coupling have dissimilar metal mating parts is provided with a grease comprising a hydrocarbon base oil containing a cationic gelling agent, particularly a Na, Li and Ba stearate. This coupling is anti-galvanic corrosive. Such couplings are useful in fire-fighting equipment where often aluminum and bronze components are in mating relation- ship, such as fire hose adaptors and hose nozzles.

331443

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Galvanic corrosion prevention coupling does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Galvanic corrosion prevention coupling, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Galvanic corrosion prevention coupling will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-846406

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.