A method and apparatus for increasing the early and long term strength of underground cemented backfills includes adding heat to the backfill. A cementitious binder is mixed with a sand component and water to form the mine backfill that may be a slurry or a paste. Heat is added to the backfill before the backfill is supplied to a mine cavity and this has been found to increase the early and long term strength of an underground cemented fill resulting from the backfill in the mine cavity. The backfill from the mixing step is mixed to have a pulp density of about 55% to 87%. Heat is added to the backfill so that the backfill has a temperature of about 18 to 60°C when it is supplied to the mine cavity. Heat is either added by heating the sand or water before the mixing step, or by heating the backfill after the mixing step. The mixing step uses a binder content of about 1.5 to 10% by weight.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Heat added to underground cemented fill to obtain both early... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Heat added to underground cemented fill to obtain both early..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Heat added to underground cemented fill to obtain both early... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1900328

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.