High-endurance superalloy for use in particular in the...

C - Chemistry – Metallurgy – 22 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

75/7.1

C22C 30/00 (2006.01) C22C 19/05 (2006.01) C22C 38/44 (2006.01)

Patent

CA 1091475

ABSTRACT OF THE DISCLOSURE The high-endurance alloy essentially contains the following percentages by weight : 0.2 to 1.9% carbon, 18 to 32% chromium, 1.5 to 8% tungsten, 15 to 40% nickel, 6 to 12% molybdenum, 0 to 3% niobium-tantalum, 0 to 2% silicon, 0 to 3% manganese, 0 to 3% zirconium, 0 to 3% vanadium, 0 to 0.9% boron, less than 0.3% cobalt and a quantity of iron such as to ensure overall balance of the alloy; this alloy can be employ- ed especially in a nuclear environment.

275142

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

High-endurance superalloy for use in particular in the... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with High-endurance superalloy for use in particular in the..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High-endurance superalloy for use in particular in the... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-220136

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.